STUDY OF SURFACE DEFECT TRANSFORMATIONS DURING PIPE MANUFACTURING USING PRP-80
Keywords:
pipe rolling, pipe-rolling blank, external surface defects, pit (dent), pipe-rolling sliver, fold, defect transformationsAbstract
Requirements of current Russian and foreign standards are becoming stricter in terms of regulating the acceptable depth of the defects located on the surface of rolled pipes. Non-conformities spoil the appearance of products, increase the risk of defects during pipe manufacturing and of pipes becoming byproducts, and degrade the competitive advantage of pipe-rolling plants with a continuous rolling mill, i.e. process yield. At the same time, quality requirements to the surface of primary hotworked or continuously cast blanks allow manufacturing-related surface defects. That is why it is necessary to examine the pipe manufacturing technology potential to reduce depth of such defects. Hot rolling modes for seamless pipes in certain PRP mills may contribute both to the defects and to the reduction of depth of blank defects. The article describes results of a complex approach to the study of defect transformation processes of the blanks rolled in ТПА-80 mills. The statistical analysis of pipe quality helped to identify the types of external pipe surface defects typical of this techology. The authors studied and defined more exactly the causes of such external surface defects as pits (dents), pipe-rolling slivers, and folds. Depending on the type of defects, they pinned down the place where they appear in the PRP mill during manufacturing tests. They also studied mechanisms of evolution of these defects from primary blank defects. Using computer-based simulation methods, they also studied the effect of technological rolling parameters on the change in geometry of defects of various shapes and initial depths. Reducing mills do not have any considerable effect on the defect depth reduction. Floating mandrel piercing and continuous rolling mills feature the widest variety of rolling adjustment parameters in ТПА-80. The authors proposed formulas to calculate defect depth reduction during the rolling process in piercing and continuous rolling mills. These formulas may be used to calculate the acceptable depth of primary and intermediate blank defects.References
STO TMK 56601056-0008-2006. Zagotovka trubnaya nepreryvnolitaya kruglogo secheniya dlya izgotovleniya besshovnykh trub. Tekhnicheskie usloviya. Standart organizatsii [Billet pipe continuously cast round cross-section for the manufacture of seamless pipes. Technical conditions organization standard]. Chelyabinsk, OJSC “RosNITI”, 2018, 29 p.
TU 0913-180-00186269-2016. Zagotovka trubnaya iz nelegirovannoi i legirovannoi stali. Tekhnicheskie usloviya [Billet pipe from unalloyed and alloyed steel. Technical conditions]. Nizhnii Tagil, OJSC “EVRAZ NTMK”, 2016, 21 p.
TU 14-104-183-99. Zagotovka trubnaya katanaya iz legirovannoi stali dlya nasosno-kompressornykh i obsadnykh trub s uvelichennym resursom ekspluatatsii. Tekhnicheskie usloviya [Alloy steel rolled billet for tubing and casing with increased service life. Technical conditions]. Novotroitsk, OJSC “NOSTA” (OKhMK), 1999, 6 p.
DIN EN 10216-1:2004. Nahtlose Stahlrohre für Druckbeanspruchungen – Technische Lieferbedingungen – Teil 1: Rohre aus unlegierten Stählen mit festgelegten Eigenschaften bei Raumtemperatur; Deutsche Fassung, 2004, 30 p. DOI: 10.31030/2401587
ASME SA-106/SA-106-M-2017. Specification for seamless carbon steel pipe for high-temperature service. ASTM International, 2017, 12 p.
TU 14-157-99-2005. Truby stal'nye besshovnye obsadnye bezmuftovye s rez'bovym soedineniem “TMK UP TMK-1” [Seamless casing steel pipes without coupling with threaded connection “TMK UP TMK-1”]. Taganrog, PJSC “TAGMET”, 2005, 25 p.
Bettayeb M., Bouali E., Abdelbaki N., Gaceb M. Establishment of a database and a classification of the defects in the metal of pipes according to their severity. Procedia Engineering, 2012, vol. 42, pp. 607–615. DOI: 10.1016/j.proeng.2012.07.453
ITS 27-2017. Proizvodstvo izdelii dal'neishego peredela chernykh metallov. Informatsionnotekhnicheskii spravochnik po nailuchshim dostupnym tekhnologiyam [Production of further redistribution of ferrous metals. Information Technology Guide on Best Available Technologies]. Moscow, Byuro NDT Publ., 2017, 402 p.
Jin R. Development of MPM Tube Rolling Technology. Baosteel Technology, 2005, p. 10–14. 10. Jin R. 17 Year’s Long History of PQF. Steel Pipe, 2009, vol. 38, no. 1, pp. 36–40.
Cernuschi E. FQM TM: Danieli 3-Roll Pass Retained Mandrel Mill for High Quality Seamless Tube Production. Iron and Steel, 2008, vol. 43, no. 12, pp. 92–95.
Pravosudovich V.V., Sokurenko V.P., Danchenko V.N. Defekty stal'nykh slitkov i prokata: spravochnoe izdanie [Defects of Steel Ingot and Rolled: Reference Edition]. Moscow, Intermet Inzhiniring Publ., 2006, 384 p.
Ovchinnikov D.V. Razrabotka, issledovaniye i vnedreniye tekhnologii proizvodstva vysokokachestvennykh nasosno-kompressornykh trub iz nepreryvnolitoy zagotovki: dis. kand. tekhn. nauk [Development, research and implementation of a technology for the production of high-quality tubing from a continuously cast billet. Cand. sci. diss.]. Ekaterinburg, 2011, 247 p.
STO TMK 56601056-0028-2013. Klassifikator defektov goryachekatanykh trub iz nepreryvnolitoi trubnoi zagotovki. Standart organizatsii [Classifier of defects of hot rolled pipes from continuously cast pipe billet. Organization standard]. Chelyabinsk, OJSC “RosNITI”, 2013, 166 p.
Minaev A.A., Zakhur M., Konovalov Yu.V. [The specifics of the use of rolled and continuously cast billets for pipe production]. Proizvodstvo prokata. Moscow, Nauka i tekhnologii Publ., 2005, no. 4, pp. 29–37. (in Russ.)
Li Sheng-Zhi, Xu Jie, Yin Yuan, Xue Jian-Guo, Feng Yuan. Mechanism of internal crack formation of seamless modified 9Cr-1 Mo steel tube rolled by mandrel mill and its application. Proceedings of Sino-Swedish Structural Materials Symposium, 2007, pp. 273–276. DOI: 10.1016/s1006-706x(08)60093-x
Chuev A.A., Danchenko V.N. [Ways to solve the problems of improving the surface quality of pipes rolled on PRP-140 with a two-stand longitudinal rolling mill]. Metallurgicheskaya i gornorudnaya promyshlennost'. Dnepropetrovsk, NII Ukrmetallurginform Publ., 2012, no. 3, pp. 49–53. (in Russ.)
Tereshchenko A.A., Kravchenko O.Yu., Skrynnik A.V., Frolov Ya.V. [Modification of defects of hot-pressed pipes during cold pilger rolling]. Plasticheskaya deformatsiya metallov, 2014, pp. 160–163. (in Russ.)
Zil'berg Yu.V., Gnezdilov B.V. [Shaping of surface defects of a workpiece in the production of pipes at PRP with mandrel mill]. Stal'. Moscow, Intermet Inzhiniring Publ., 1984, no. 9, pp. 59–61. (in Russ.)
Bogatov A.A., Pavlov D.A., Nukhov D.Sh. Vintovaya prokatka nepreryvnolitykh zagotovok iz konstruktsionnykh marok stali [Screw rolling of continuously cast billets from structural steel grades]. Ekaterinburg, Ural University Publ., 2017, 164 p.
Erzhanov, A.S. Optimizatsiya parametrov listovoy prokatki nizkouglerodistykh staley na osnove obespecheniya vykatyvayemosti poverkhnostnykh defektov: dis. kand. tekhn. nauk [Optimization of the parameters of sheet rolling of low-carbon steels based on ensuring the rolling out of surface defects. Cand. sci. diss.]. Termitau, 2016, 145 p.
Bogatov A.A., Pavlov D.A., Lipnyagov S.V., Suvorov V.N. [Modeling the formation of a “groove” defect on the inner surface of pipes during longitudinal rolling]. Proizvodstvo prokata, 2012, no. 8, pp. 37–39. (in Russ.)